Item | Fireclay | High Alumina | High Mullite | Corundum | ||||||
NP-45 | LP-55 | LP-70 | MP-55 | MP-70 | MP-45 | GP-60 | GP-70 | GP-90 | ||
AL2O3(%) | ≥45 | ≥55 | ≥70 | ≥50 | ≥50 | ≥50 | ≥50 | ≥50 | ≥50 | |
Flexural Strength (MPa) |
110℃ | ≥2.0 | ≥2.0 | ≥2.0 | ≥2.0 | ≥2.0 | ≥2.0 | ≥2.0 | ≥20 | ≥2.0 |
After high-temperature burning | ≥5.9 | ≥5.9 | ≥5.9 | ≥5.9 | ≥5.9 | ≥5.9 | ≥5.9 | ≥5.9 | ≥5.9 | |
1200℃ | 1400℃ | 1400℃ | 1400℃ | 1500℃ | 1350℃ | 1400℃ | 1500℃ | 1500℃ | ||
Refractoriness(℃) | ≥1700 | ≥1750 | ≥1790 | ≥1770 | ≥1790 | ≥1700 | ≥1790 | ≥1825 | ≥1850 | |
Refractoriness under load(T2℃) | ≥1200 | ≥1250 | ≥1300 | ≥1400 | ≥1500 | ≥1350 | ≥1550 | ≥1550 | ≥1700 | |
Bonding time/min | 1~2 | 1~2 | 1~2 | 1~2 | 1~2 | 1~2 | 1~2 | 1~2 | 1~2 | |
Reheating Linear Change Rate(%) | 0~+1 1400℃x3h |
|||||||||
Granularity | ≥0.5mm | ≤1.0 | ≤1.0 | ≤1.0 | ≤1.0 | ≤10 | ≤1.0 | ≤1.0 | ≤1.0 | ≤1.0 |
≤0.076mm | ≥50 | ≥50 | ≥50 | ≥50 | ≥50 | ≥50 | ≥50 | ≥50 | ≥50 |