Product Introduction:Vermiculite Insulation board, commonly known as insulation board or refractory board, is a new type of insulation material. It is a board made of expanded vermiculite and a certain amount of adhesive, which is hot pressed or cold pressed.
Product Highlights:- High temperature resistance, excellent fire resistance
- Perfect sound insulation performance
- Environmental protection, even heating up to 1200 ℃ does not produce harmful gases to human health
-
Application:Vermiculite insulation board is widely used abroad in fields such as construction, shipbuilding, metallurgy, power, aerospace, etc.
Technical Data:
Item |
Index |
Length & width |
1200×1000 mm |
Thickness |
10-50mm |
Density |
350kg/m³-1250kg/m³ |
Specifications |
VM-450 |
VM-550 |
VM-1100 |
VM-1250 |
Features |
Index |
Unit |
Index |
Unit |
Index |
Unit |
Index |
Unit |
Maximum service temperature |
1100 |
°C |
1100 |
°C |
1100 |
°C |
1100 |
°C |
Bulk density |
450 |
Kg/m3 |
550 |
Kg/m3 |
1100 |
Kg/m3 |
1250 |
Kg/m3 |
Cold crushing strength |
2.5 |
MPa |
3.5 |
MPa |
8.5 |
MPa |
8.5 |
MPa |
Modulus of rupture |
0.3 |
MPa |
1.2 |
MPa |
2.5 |
MPa |
2.5 |
MPa |
Linear reheat shrinkage after 12 hours at 1000°℃ |
1.0 |
% |
1.0 |
% |
1.5 |
% |
1.5 |
% |
Total porosity |
80 |
% |
76 |
% |
53 |
% |
55 |
% |
Coefficient of reversible thermal expansion at 20°℃ to 750°℃ |
11 |
X10-6K-1 |
11 |
X10-6K-1 |
10 |
X10-6K-1 |
10 |
X10-6K-1 |
Resistance to thermal shock |
>30 |
Cycles |
>30 |
Cycles |
>30 |
Cycles |
>30 |
Cycles |
Thermal conductivity |
Mean temperature |
|
|
|
|
|
200℃ |
0.10 |
W/(m×K) |
0.10 |
W/(m×K) |
0.09 |
W/(m×K) |
0.08 |
W/(m×K) |
|
400℃ |
0.11 |
W/(m×K) |
0.12 |
W/(m×K) |
0.15 |
W/(m×K) |
0.14 |
W/(m×K) |
|
600℃ |
0.13 |
W/(m×K) |
0.13 |
W/(m×K) |
0.19 |
W/(m×K) |
0.18 |
W/(m×K) |
|
800℃ |
0.16 |
W/(m×K) |
0.17 |
W/(m×K) |
0.21 |
W/(m×K) |
0.20 |
W/(m×K) |
|
Chemical |
Index |
Unit |
Index |
Unit |
Index |
Unit |
Index |
Unit |
SiO2 |
51 |
% |
49 |
% |
50 |
% |
52 |
% |
TiO2 |
1.6 |
% |
1.7 |
% |
2.5 |
% |
1.6 |
% |
Fe2O3 |
3.6 |
% |
3.6 |
% |
4.7 |
% |
3.6 |
% |
Al2O3 |
24 |
% |
26 |
% |
23 |
% |
23 |
% |
MgO |
8.9 |
% |
8.8 |
% |
8.9 |
% |
8.9 |
% |
CaO |
1.5 |
% |
1.5 |
% |
1.5 |
% |
1.5 |
% |
Na2O |
0.2 |
% |
0.2 |
% |
0.2 |
% |
0.2 |
% |
K20 |
5.6 |
% |
5.6 |
% |
5.6 |
% |
5.6 |
% |
LOI at 1,025℃ |
6.0 |
% |
4.0 |
% |
3.0 |
% |
2.8 |
% |